Loan If you have an assembly that can be cleaned in and in-line aqueous cleaner (no moisture sensitive parts). Then using DI water and a saponifier called EnviroGold 816 at 5% (wash temperatue 130-145 F) with low pressure sprays (25-30 psi) will completely remove the finger prints and any trace of who done it. This could be brushed on and rinsed in an in-line aqueous cleaner as well. This saponifier has great flux and residue removing capabilities. The contact for this material is Mark Palmer at EnviroSense (408)894-9901 Terry Munson [log in to unmask] CSL Inc. 765-457-8095 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################