In a message dated 5/7/99 3:00:30 PM Pacific Daylight Time, [log in to unmask] writes: << As many of you, I have been concerned and questioned voiding % and volume plus all the rest. However, I keep coming back to one thing haunting. What's in the voids? In other times, I found horrific problems with residual flux entrapped in the voids. This often was effected by solder termination area contamination. The flux remained in the joint trying to do what was intended - fight the infection. Often, this resulted in failures as the solder joint continued to fail as it was "erroded" away. Certainly, X-Ray points the way to what is to be X-Sectioned. Beyond that, some type chemical analysis technique needs to examine the residue left in the void. I have graphic evidence of this phenomonom as, probably, do most of you. Does this continue to be an issue in the BGA world as it did/does in the PLCC/QFP arena? Earl Moon >> Hi ya Earl! Haven't heard from you inna while...was wondering when you'd get back into the fray! Anyways, about these voids. On the ones that you have found contaminated with something, where were they? Up inside the ball, or more down towards the ball/pad interface? It goes back to how the void was created in the first place. I've read and heard that many times you stand a very good chance of creating voids if your reflow profile isn't what it needs to be, and that seems pretty logical to me. Perhaps if you don't give yourself enough time to drive all the volatiles off the way you should, and then spike the crap out of the board, zoom it out of the oven to cool down quickly, I can see where you would have a good chance of creating a bubble or two inside the joints. To me, a good sized BGA with it's connections buried deep inside beneath the body is going to take quite a bit longer to have all the volatiles driven off the way a gull wing part or "J-leaded" part does, simply because the interior of the BGA is not getting the benefit of the convection heating and swirling air he way the other parts do...it's getting it's heat from the radiation of heating package body and the PCB...am I off base here? So what I'm saying, is that maybe you need to stretch the profile out for a longer period of time on a board that has BGA's on it so you can be sure that all of the volatiles are driven off, and that you've given enough time to truely preheat things thoroughly. Instead of the normal 4.5 to 5 minute profiles that most of us are used to, maybe it should be more like 5 to 6 minutes or whatever...heck, I'm just thinking out loud here. I just think that instead of worrying how big a void can be and live with it when you see it in a x-ray, we need to really figure out what's causing them and not do that anymore...then we won't need an x-ray. I can't afford one anyway...you guys get all the fun toys! (sniff, sniff....) -Steve Gregory- P.S. Did any of you check out that ERSA inspection system that Paul told ya' about? ( http://www.ersa.de/inspec.htm ) I'd take a look at it if I were you...no kidding, it's one of the coolest pieces of inspection equipment I've ever seen! ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################