Hi Mike,
in response to your mail, I still am wondering how EPO-TEK can insist
that helium leakage rate of 1x10exp-8. Such low rates use to be obtained
in metal housings only. If, I say, if the rate is such low, then you
meet the military specs, and accordingly, you can seal with H77. It's a
serious temptation, isn't it? /Ingemar Hernefjord
----------------------------old messages------------------------------
> In a message dated 11/05/99 09:16:19AM, you write:
>
> > To: [log in to unmask]
> >
> > Hellouu.
> > EPO-TEK H77 is hermetic. At least according to their databook:
> > 1.0x10exp-8 cc/sec Helium. Excellent for sealing MCMs and other
> > packages, they say. Now, why do we laserweld, seamweld or solder
metal
> > cans if you can just use H77? We are old byuers of EPO-TEK and we
like
> > them, but this question has to be ventilated: can a "plastic"
really be
> > that tight against Helium? Or worse...against Hydrogene? A teacher
at
> > one of our universities (chemistry professor) said that 'an organic
seal
> > can never,never and never be hermetic'. Time for revolution? If the
MIL
> > people really accept e.g. H77 as a sealant, I think it's kind of
smash!
> > We can creep out of the cave and drop the club!/
> > Ingemar Hernefjord
> > Ericsson Microwave Systems
>
> Hermetic is one of those words which can mean what you want it to
mean. As
> used in top whack space or MIL spec connotations conventional wisodm
is that
> organic compounds can not be Hermetic with a capital H, because their
> molecular density is too low and anyway there is always an interface
which
> acts as a conduit for moisture. H77 has been around a long time and
its
> almost as long since I looked at it and the claim in detail. So far as
I
> recall the xplanation for the claim for hermeticity is explained
something
> like this: there are/were several test procedures in MIL601 of
differing
> severity and the one which most people think of is the hardest,
overlooking
> the less severe ramps etc in other test methods under the spec. H77
meets a
> less severe case. This is not to say that H77 is without merit, it all
> depends on what you mean by Hermetic and what you actually need....
>
> Mike Fenner
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text
> in the body:
> To subscribe: SUBSCRIBE TechNet
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
> ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################