Forwarded message: From: Self <SWFN01/PDIAMOND> To: [log in to unmask] Subject: Ultrasonic soldering Reply-to: [log in to unmask] Date: Fri, 7 May 1999 08:15:42 EMT+0 Hello all, I have just been reading an article on Ultrasonic soldering which looks interesting, has anyone out there had had any experience of this process? Thanks, Pat Diamond Weston Aerospace Pat Diamond Senior Manufacturing Engineer Weston Aerospace Farnborough Hampshire GU14 7PW Tel 01252 544433 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################