Hi Werner Thanks for your feedback on rework reliability data. FYI - John Goldak is a Professor at Carleton University in Ottawa, Canada who is doing some FET development in solder joint thermal stress reliability. His equations are unique in that they account for the transient temperature gradient within the BGA package and relaxation creep. He claims that the FET program will run on a Pentium II 400 MHz in less than five hours. I suggest that you contact him directly at [log in to unmask] for a more detailed explanation. Dan Gilpin Process Engineering Mitel Corporation ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################