On 05/28/99 20:02:12 you wrote: > >Ed, > >Your 2 cents worth really got me excited. > >I attempted to ultrasonic cleaned in a (Alkaline, PH 8 to 9) neutraliser >for 15 mins but the stubborn white contaminants still remained. > >I shared your sentiment and am suspecting the contaminants to come from the >solder. The supplier will help analyse in their lead content on the same >batch used in production. > >Could you elaborate the effects of low antimony? > >Thanks for sharing. > David, First, it seems to me that analysis of your solder pot is not a regularly scheduled item. Several contaminants can be intoduced from the PCB's and other misc. sources such as fixtures, tools, etc. You should not only test for lead content(actually tin content, balance lead), but other metals such as copper, gold, silver, nickel, bismuth, antimony, zinc, cadmium, aluminum, arsenic, iron, etc. (I did this from memory, so I probably missed a few). QQS571 spells out the upper and (in a few cases) lower limits. Antimony has a peculiar property in that it expands when cool and contracts when heated. I believe bismuth is used in the equation as well, but not being a metalurgist, I am simply repeating what I've been told, contaminated by an aging memory (it's the second thing to go, I've also been told... I think.) The effect is as the surface cools and freezes, the body of the joint is somewhat lagging thermally, therefore contracting after there is a skin formed causing "wrinkles" (another sign of aging, by the way). Antimony reduces the shrinkage in this interim stage. Regards, Ed Popielarski QTA Machine 10 Mc Laren, Suite D Irvine, Ca. USA 92618 Ph: (949)581-6601 Fx: (949)581-2448 E-Mail: [log in to unmask] http://www.qta.net ASK ABOUT OUR BGA REBALLER! ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################