Hello Technetters, This is the IPC definition Regarding solder ball acceptability, IPC-A-610B, "Acceptability of Electronic Assemblies," section 4.1, states: Nonconforming Defect - Class 1, 2, 3 Solder balls/splashes violate minimum electrical design clearance, or are not encapsulated imbedded in a permanent coating or attached to a metal contact. Nonconforming Process Indicator - Class 1, 2, 3 Solder balls/splashes which are within 0.13 mm of lands or traces, or exceed 0.13 mm in diameter. More than 5 solder balls/splashes (0.13 mm or less) per 600 sq. mm. Please explain the meaning of the above sentence. Dose (0.13 mm or less) related to the Solder Balls diameter or 0.13 mm of lands or traces Dose it mean that 5 solder balls/splashes that are bigger then 0.13 mm are acceptable or it mean that 5 solder balls/splashes that are more then 0.13 mm of lands or traces are acceptable. Maybe we gut it all wrong please advice. Best Regards Chaim Krief Process Engineer Motorola South Israel Ltd. 16 Hakodhim St., Industrial Zone P.O.B. 509 Arad 89104, Israel Tel: +972-7-9970344 Fax: +972-7-9970327 [log in to unmask] <mailto:[log in to unmask]> ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################