Hello Rich! There are in fact several alternatives to black oxide. Among them are Double Treated copper foils, which are readily available in both standard and reverse-treated versions. Don't hesitate to contact me if you would like more information. Jonathan Meigs Product Development Engineer -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Thursday, May 06, 1999 11:32 AM To: [log in to unmask] Subject: [TN] Black oxide process In producing multilayer PCB's, there is an oxide process used to prevent pink ring. Usually this process is called the "black oxide process" and requires use of a reducer solution containing an amine borane. Is this process considered a standard in the PCB industry and is it's use increasing? Are there alternative processes which accomplish the same objective? What is the future trend to eliminate pink ring? ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ begin 600 Meigs, Jonathan.vcf M0D5'24XZ5D-!4D0-"E9%4E-)3TXZ,BXQ#0I..DUE:6=S.TIO;F%T:&%N#0I& M3CI-96EG<RP@2F]N871H86X-"D]21SI!;&QI9613:6=N86P@+2!%;&5C=')O M;FEC($UA=&5R:6%L<PT*3D]413I0+D\N($)O>"`Y.0T*5$5,.U=/4DL[5D]) M0T4Z*#4Q."D@-C@V+30Y-C$-"D%$4CM73U)+.CM/86L@36ET<W5I.S@P($9I M<G-T(%-T<F5E=#M(;V]S:6-K($9A;&QS.TY9.S$R,#DP.U53#0I,04)%3#M7 M3U)+.T5.0T]$24Y'/5%53U1%1"U04DE.5$%"3$4Z3V%K($UI='-U:3TP1#TP M03@P($9I<G-T(%-T<F5E=#TP1#TP04AO;W-I8VL@1F%L;',L($Y9(#$R,#DP M/3!$/3!!55,-"D5-04E,.U!2148[24Y415).150Z2F]N871H86XN365I9W-` M06QL:65D4VEG;F%L+F-O;0T*4D56.C$Y.3DP-#$R5#$U-#DS-UH-"D5.1#I6 &0T%21`T* ` end ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################