I have gotten them from Hunter Products, 792 Partridge Drive, Bridgewater, NJ 08807 (908) 526-8440. Mike McMonagle PCA Process Engineering Supervisor K*Tec Electronics 1111 Gillingham Lane Sugar Land, TX 77478 (281) 243-5639 Phone (281) 243-5539 Fax [log in to unmask] > -----Original Message----- > From: Paul Peltier [SMTP:[log in to unmask]] > Sent: Friday, April 23, 1999 1:45 AM > To: [log in to unmask] > Subject: [TN] plating pens > > CAN ANY ONE GUIDE ME TO A SUPPLIER OF PLATING PENS INTENDED FOR GOLD > EDGE FINGER CONNECTOR REPAIR. > I HAVE PURCHASED THESE PENS IN THE PAST, BUT NOW CAN'T SEEM TO > REMEMBER > I PURCHASED THEM. > ALL RESPONSES WILL BE GREATLY APPRECIATED. > > THANK YOU > > PAUL > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################