From: Dennis J Fall@TFT on 04/20/99 03:06 PM To: [log in to unmask] cc: Subject: Electrolytic plating on isolated areas or an alternative I have been pulling my hair out trying to figure out how to electroplate solder onto isolated areas (land pads, etc.). I have also been trying to come up with other ways to do this (immersion, etc.). I basically need about 5 ?m (0.2 mils) of solder. Does anyone have any great ideas??????? Thank You, Dennis Fall P: 507-625-8445 x17 Engineer F: 507-625-3523 Thin Film Technology Corporation mailto:[log in to unmask] 1980 Commerce Drive http://www.thin-film.com North Mankato, MN 56003-1702 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################