Chris is right. It is not a good idea to strip resist in caustic when there is solder or tin present. Most proprietary strippers contain Monoethanol Amine (70-80%) and 1,2 Ethanediamine (5-10%) and trace amounts (1-5%) of anti-tarnish like Benzotriazole to keep the copper bright. In a previous life we used generic Monoethanolamine as a resist stripper. It can be a bit malodorous (smells like dead fish) but it gets the job done. The waste stripper is pH neutralized to precipitate out the resist and then treated for dissolved metals if necessary. There should be much less dissolved metal than a caustic styripper because the amine based strippers do not remove as much metal from the boards. > -----Original Message----- > From: Albert Mok [SMTP:[log in to unmask]] > Sent: Saturday, April 10, 1999 6:44 AM > To: [log in to unmask] > Subject: [TN] Problem during strip dry film > > Dear team, > > We have problem during dry film stripping, which is the process just > before > etching. > > During the dry film stripping, two stages of dry film stripping processes > are used and some of the Tin(act as etch resist) seems dissolve a bit at > the bare copper area just after stripping when in contact with stripping > solution of caustic soda and result etching problem. Especially for fine > spacing of 6-8mil, the incomplete etching problem are more serious and > sometimes re-etch the boards for twice again are required. > > Do anyone have any idea to resolve it? The temperature employed is 40 C > and the conc. of NaOH is 150 g/L. > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################