David Not sure why Europe would want a high CTI rated laminate more so than any other region. There have been past posts on this subject but the gist of it is that for circuits carrying high power, the higher the laminate CTI rating the closer the etch spacings that regulatory agencies permit. I don't believe this was ever mentioned in past posts but this is the primary reason for even considering CTI ratings in the first place. Most situations do not care about laminate CTI rating as the laminate vendors correctly point out. Other postings describe the CTI test methodology so I won't go into that. As for materials with high enough CTI ratings, most epoxy based materials have relatively the same CTI ratings. The individual differences are not significant enough. Solely from my memory, which fails me every now and then, I remember that the polyester based materials have higher CTI than epoxies. I also remember that several years ago, Hitachi offered a laminate that was made from a copper foil which had a thin ceramic layer blasted onto the back ( i.e. tooth ) side. This material had phenomenal CTI values due to the ceramic layer. Good luck. /Gerry -----Original Message----- From: Bay State Circuits, Inc. [mailto:[log in to unmask]] Sent: Friday, April 16, 1999 9:47 AM To: [log in to unmask] Subject: [TN] Comparative Tracking Index (CTI) on Circuit Board Material Dear Techntters I have a customer that is looking for ciruit board material that has a CTI rating of 400 and one of 600. Most of the techs from the laminate manufacturers respond with Who cares about CTI? It seems my customer is getting this pressure from their customers in Europe. Can anyone tell me why Europe is concerned with that high a CTI and can anyone tell me where I can get material with that high a CTI rating? I have tried some of the well known manufacturers (Allied, GE, PolyClad) with no luck. Thank you David ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################