In a message dated 3/24/99 5:08:27 PM Pacific Standard Time, [log in to unmask] writes: > Kathy, > > I can't speak much to the silver migration issue, but I whole-heartedly > concur with Steve's comments regarding manufacturability. We've used these > parts extensively on boards we build for several customers, and have found a > significant increase in shorts on the convex parts. > > Rick Thompson > Ventura Electronics Assembly > 2665A Park Center Dr. > Simi Valley, CA 93065 Hi Kathy, In thinking about things, it was over three years ago that I worked at that memory company that I spoke of...we could find out right here if there's a silver migration issue with concave terminations... Out of these 5 computer companies; Hewlett Packard, Dell, IBM, Compaq, or Toshiba, how many of you as owners or operators, have had problems with their cache memory? Not saying that we built memory for all of these companies, ...or three,....or two,...or? But we did at least one of them (just covering my fanny here). But seriously, has anybody?....didn't think so... These are the "big boys", and I'm sure that if there was a problem with the silver migration issue, we would have heard something about it. I've got documents from Phillips component engineers who did a study and recommended using concave chip networks over convex ones...now why would they do that if there was a problem? I suspect that it's easier and cheaper to make them convex than concave (I'm just guessing though), and the demand is rising for concave ones since everybody is learning how much better they solder than the convex ones do... What am I thinking? Salesmen don't do things like that, now do they?...'scuse me for my outburst... -Steve Gregory- ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################