Jeff, MInimum Ni thickness requirements vary depending on the requirements the end product must meet. The nickel's main purpose is as a migration barrier between the substrate metalizations and gold . In most cases 100 - 200u" of nickel is sufficient. (as a matter of fact most part specifications I've worked with for gold finishes request nickel thicknesses in this rannge). Take care, Bruce Stacy JEFF PERKINS <[log in to unmask]> on 03/03/99 09:45:24 AM Please respond to "\"TechNet E-Mail Forum.\" <[log in to unmask]>, JEFF PERKINS" <[log in to unmask]> To: [log in to unmask] cc: (bcc: Bruce Stacy/ECSDOMAIN) Subject: [TN] Minimum Ni thickness We have a ceramic submount where the finish metallization is Ni-Au. Interconnects are formed from a AuSn solder and Au wirebonds. Does anyone have pointers to specifications for minimum Ni thickness? Thanks, Jeff Perkins Epitaxx (UUEncoded file named: att1.htm follows) (Its format is: Internet HTML ) begin 644 att1.htm M/"%$3T-465!%($A434P@4%5"3$E#("(M+R]7,T,O+T141"!(5$U,(#,N,B\O M14XB/@T*/$A434P^#0H\2$5!1#X-"CQ-151!($A45%`M15%5258](D-O;G1E M;G0M5'EP92(@0T].5$5.5#TB=&5X="]H=&UL.R!C:&%R<V5T/75S+6%S8VEI M(CX-"CQ-151!($Y!344](D=E;F5R871O<B(@0T].5$5.5#TB35,@17AC:&%N M9V4@4V5R=F5R('9E<G-I;VX@-2XU+C(R,S(N,"(^#0H\5$E43$4^36EN:6UU M;2!.:2!T:&EC:VYE<W,\+U1)5$Q%/@T*/"](14%$/@T*/$)/1%D^#0H\0E(^ M#0H-"CQ0/B9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R9N M8G-P.R`\1D].5"!325I%/3(@1D%#13TB07)I86PB/E=E(&AA=F4@82!C97)A M;6EC('-U8FUO=6YT('=H97)E('1H92!F:6YI<V@@;65T86QL:7IA=&EO;B!I M<R!.:2U!=2XF;F)S<#L@26YT97)C;VYN96-T<R!A<F4@9F]R;65D(&9R;VT@ M82!!=5-N('-O;&1E<B!A;F0@074@=VER96)O;F1S+B9N8G-P.R!$;V5S(&%N M>6]N92!H879E('!O:6YT97)S('1O('-P96-I9FEC871I;VYS(&9O<B!M:6YI M;75M($YI('1H:6-K;F5S<S\F;F)S<#L@/"]&3TY4/CPO4#X-"@T*/%`^)FYB M<W`[)FYB<W`[)FYB<W`[)FYB<W`[)FYB<W`[)FYB<W`[)FYB<W`[(#Q&3TY4 M(%-)6D4],B!&04-%/2)!<FEA;"(^5&AA;FMS+#PO1D].5#X-"CQ"4CXF;F)S M<#LF;F)S<#LF;F)S<#LF;F)S<#LF;F)S<#LF;F)S<#LF;F)S<#L@)FYB<W`[ M)FYB<W`[)FYB<W`[)FYB<W`[)FYB<W`[(#Q&3TY4(%-)6D4],B!&04-%/2)! M<FEA;"(^2F5F9B!097)K:6YS/"]&3TY4/@T*/$)2/B9N8G-P.R9N8G-P.R9N M8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R`F;F)S<#LF;F)S<#LF;F)S M<#LF;F)S<#LF;F)S<#L@/$9/3E0@4TE:13TR($9!0T4](D%R:6%L(CY%<&ET M87AX/"]&3TY4/@T*/$)2/B9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P.R9N8G-P M.R9N8G-P.R9N8G-P.R`F;F)S<#LF;F)S<#LF;F)S<#LF;F)S<#LF;F)S<#L@ <#0H\+U`^#0H-"CPO0D]$63X-"CPO2%1-3#X-"F5A ` end ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################