Hello everyone,

I have been doing tensile testing on a veriety of solders and find that at
the crosshead speed I am using makes the Sn-40Pb solder superplastic.

Do any of you have information on the strain rate sensitivity of solders?
Most suggestions will be appriciated.

Thank you
Tamara E. Bloomer
Assistant Scientist
Iowa State University
Ames Laboratory
137 Wilhelm Hall
Ames, Iowa 50011
[log in to unmask]