Hey Graham - Thanks for the addition - like you, I'm a little leery of what the "expert" said, or at least the words used in the media to describe what they thought he said. Not that this could not have occurred, but it sounds like and awful lot of supposition, with no indication that supports established fact. In my recollection, the U.S. military "limited usage" rather than "banned usage". There is, and has been for many years, a limitation on PTFE jacketed wire as a result of its cold flow charactaristics. Guess I've gotten somewhat skeptical since I've grown into geezerhood. Y'all have a fun day - Kelly ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################