Hi, Teo: Our comapany produces a microetchant/cleaner for use in the fabarication of multi-layer printed wiring boards. It is a H2SO4-H2O2 based formula. It takes about 10-20 seconds in dip or spray application to remove all fingerprints, copper oxides, grease, chromate, arsenate and zinc. The etch rate can be easily controlled by the concentration of H2O2 added. The H2O2 in the solution is also very stable in the solution. If you allow the bath to open in the air (no microetchant/cleaner application)for a month, you are likely to see an increase in the H2O2 concentration. If you would like to have a sample for a test, please send me your address to [log in to unmask] Gary -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask] Sent: Wednesday, February 03, 1999 10:18 AM To: [log in to unmask] Subject: [TN] Looking for OFHC copper and cleaner My company is located in El Paso, and I cannot find any local lab supply stores that have "Oxygen Free High Conductivity (OFHC)" copper (75 mm X 25 MM X 1 MM). Does anybody know who supplies these coupons? Also, I am trying to find some liquid copper cleaner. Your assistance would be appreciated. -Thank you, Teo Tijerina ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################