Andrew Sherry asked: >Can anyone tell me the pull-test requirement for solderless wirewrap, i.e. >frequency, tools required, procedure etc.. Use a manual pull force gage like the Wagner FDL, and a home-made metal "fork" to slip under the first wrap. Based an old copy of Bell System Practics section 800-612-154 paragraph 3.29, minimum inspection force without visible displacement is: 24 AWG 2,500 g 26 AWG 2,220 g 28 AWG 1,750 g 30 AWG 1,200 g See also Bell Communications Research publication 48010 if this is still published. I would suggest sample wraps be tested weekly for each bit/sleeve used, but this is also a function of the corner radius of the wrapped post, so you need a provision for testing normal product, or at least samples thereof. Cooper Tools of Cheraw, SC was the successor to Gardner Denver, who claims to be the inventor of this technology. Contact me for more details, I wrote a comprehensive tome on the subject of solderless wrapped connections, tooling, and maintenance for a former employer in 1991, and kept it for some bizarre reason. regards, Jerry Cupples Interphase Corporation Dallas, TX USA http://www.iphase.com ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################