Almost anything but 7628 or 29 works fine. This means relatively resin rich facing as 2113, 2116, and our favorites 1080 or 106 that all can be "sandwiched" around the 28/29 stuff. You have lots of room to work with in an MLB .125" thick so there should be no problems with many alternatives indicated. Earl Moon ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################