Surprised Steve The Legend did not cover this one for you Rich . Gettin' slack with that swollen head . Or maybe he went for that soak ? Anyhow ; one of Multi's better products is their peelable latex ; I think they call it Spot On . It pulls out very easy even when embedded deep in barrels . However if it is the peel from fab's ; yo're dun in for ; not much you can do . The sugg. would be ; if you have fab's peel that is ; drop it from order and do it in-house if you have racking for it ; takes 5 mins to touch dry . That's what we did ; same here ; the blue stuff we'd have to chisel off ; apart from other troubles (packing) ; girls refused to sacrifice their classy nail jobs on it See you Paul Klasek http://www.resmed.com > ---------- > From: Hamilton, Richard -4454[SMTP:[log in to unmask]] > Sent: Friday, 5 February 1999 6:30 > To: [log in to unmask] > Subject: [TN] Peelable mask > > Hello all, > > I wanted to get a 'heads up' on a possible problem so I asked this several > months ago and got no reply. I thought, Great! This is not a problem!! > > Well, not so sure now. The peelable masking we are using on our PWB's > seems > to be getting tougher to remove after reflow process has been added to the > system. > > Anyone have any suggestions, guidelines, or other input on what to look > for > or what to look out for? We will have to start looking at other vendors > for > the masking. Sorry but I cannot tell you the mfgr right now, our PWB > designer is out today. If this information is needed, let me know and when > I > get it I will let you know. > > Thanks gang. > > Richard Hamilton > Clemar Mfg. / Rain Bird > [log in to unmask] > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################