Check into the sharpness of the tool you are using to help the breakaway become cut off. Otherwise, check with your boardhouse as to what to do to ensure that the webbing or the thin channel between the breakaway and the PCB breaks off without inflicting damage. At 04:04 PM 2/22/99 -0800, you wrote: >Tech world, >Got a problem with removing breakaway tabs. When we remove them, the >masking is peeling off with the breakaway and some times it runs into >the traces. I started to blame the assemblers, I thought they were being >to ruff but when it came time for me to remove the tabs the same thing >happen to me. Has anyone ran into this problem and if so what is the >root cause. Any help would be appreciated. > >Thanks >Angie Marques >Quadrus >408-918-5045 > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################