Navin, I think you will struggle with this - the V grooves in Si are formed by anisotropic etching, which is not possible with an amorphous materials such as glass. David Whalley Loughborough University At 10:13 AM 2/16/99 -0000, Navin Suyal wrote: >Hi Everybody, > >I am searching for V-grooves compatible with multimode fibers on >glass (silica or any other glass) substrates. All the producers I >could find so far, supply V-grooves on Silicon. Could anybody >inform me about the suppliers of V-Grooves on glass. > >Thanks in advance, > >Navin Suyal > >Navin Suyal >Optical Computing and Interconnects Group >Dept. of Physics | Tel. 0044-131-451 3068 >Heriot-Watt University, | Fax 0044-131-451 3136 >Edinburgh, EH14 4AS (UK) | e-mail [log in to unmask] > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################