Excuse the late response but here is my opinion on the tests you mentioned. The halide content determination, copper mirror test, electromigration, silver chromate paper test, etc., are useful when developing a new flux. If a flux do not passes the test, there is a big risk for that it may cause reliability problems of an assembly. However, passing the tests is no guarantee for that there will be no reliability problems. That is the reason for that SIR testing is performed. It is the only test that could be characterised as a reliability test. Since the SIR on a PBA will be affected by practically all materials and processes used for the production, evaluating the impact on SIR of a flux on a bare test coupon with just a comb pattern, as is done during qualification of a flux by flux manufacturers, is not enough. Instead, SIR should be evaluated using a procedure as that described in Appendix D (Material and Process Compatibility Testing) in IPC´s standard J-STD-001B, i.e. using a test vehicle representing the substrate materials, assembly materials, and fabrication processes and measuring the SIR between solder joints to components with open circuit. If you have done that, and passed the test, I do not see any reason for that you should worry about the halide content. Per-Erik Tegehall IVF SWEDEN Phone: +46 31 706 61 48 Fax: +46 31 27 61 30 Email: [log in to unmask] > ---------- > > Dear colleagues, > > We would like to rationalise our PBA materials (solder pastes, flux) > qualification procedures. Our question is: > What is the added value of tests/measurements like halide content > determination, > copper mirror test, electromigration, silver chromate paper test, > etc., > when one does a Surface Insulation Resistance (SIR) test? What do they > tell more about the final product reliability? Does the SIR test not > cover it all? For example, should we be worried about the halide > content when the material passes the SIR test? > > We welcome any comment. > > Geert Willems > Alcatel Bell > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################