In a message dated 1/22/99 7:56:42 AM Pacific Standard Time, [log in to unmask] writes: << Hi, We use the Voltronics JS100 variable capacitor on some of our products. Recently we have encountered failures - mode is device open. On inspection it was found that the ceramic substrate was cracked on many devices where the metal frame is crimped. Inspection of devices still on the reel shows the same problem. Is anyone else using this part and having the same problem? Bob Smith Quality Engineer >> Hi Bob, I'm having problems as well with a variable capacitor, but the one I'm using is a Sprague/Goodman cap. It's about the size of a 1206 and supposedly it's able to be processed like any other SMT part. But the last batch of boards we built for our customer that used that cap said that almost every one of them failed...same mode as you. In fact, they sent me a change for us to hand solder them with no clean as a last step, and not to run them through a cleaner. I noticed your post, and got some of the caps we're using from the reel I have. Looked at about 5-10 of them under a scope, but didn't see any sort of cracking. Our customer sent me the application notes for the cap and I didn't exceed any of them when I last built their boards. The processing guidelines are: Preheat 140° ±10° C. for 2-mins., then don't exceed 240° ±5° C for 20 secs. maximum. Recommend water soluble fluxes, and water wash with, or without saponifier at fairly low temperatures (their words). I followed all the guidelines, and they still fail. I'm gonna hand solder em' this next run of boards and we'll see what happens... -Steve Gregory- ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################