Please delete my address from this list. Regards [log in to unmask] > ---------- > From: Guenter Grossmann[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;Guenter Grossmann > Sent: Friday, 22 January 1999 22:31 > To: [log in to unmask] > Subject: [TN] Dewetting on NiAu > > Hi all > > I have a request of a company working with us. They face the problem that > their solder joints of QFP's on NiAu pad surfaces ( Au electroless plated > ) > does not bond in the reflow process. Trials have been made with various > suppliers of PCB's, all with the same result. All the other components > seem > to solder Ok. Has somebody else gone through this? Does somebody know the > reason for the problem and maybe a solution? > Thanks for your help. > > Best regards > > > Guenter > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################