John To be sure it is clean under the BGA, do some ion chromatography testing (remove the BGA manually, and examine the area under the bga). IMHO, it is the only way to be sure you can clean sufficiently. If you don't have in-house capability, there are many labs that can do this sort of test for you, and recommend improvements to your process where required. Two labs I've used are: Contamination Studies Laboratory (CSL in Kokomo, Indiana, (765) 457-9033) Celestica's lab in Toronto, Canada - see their web site www.celestica.com, section on failure analysis. Once you are sure your process is a good one the use of an Ionograph or similar device is a good way to be confident you are continuing to do a good job. Good luck! Graham Collins Process Engineer, Litton Systems Canada, Atlantic Facility (902) 873-2000 ext 6215 -----Original Message----- From: John Chandler [mailto:[log in to unmask]] Sent: Monday, January 25, 1999 2:46 AM To: [log in to unmask] Subject: [TN] BGA clean checking As you all know. We are getting into doing a basic BGA assembly. The new question which came up is, since we run a water soluble flux paste. How are we going to know if it is clean under the BGA?? Any suggestions beside going to a no clean paste?? Thanks in advance. John ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################