Steve, Check out Circuit Technology Corporation, formerly known as Circuit Repair Corp, at www.circuitnet.com. They have everything you need in plating solutions/systems and fab repair supplies. They have been around forever, and specialize in just such stuff. They also have a 200 page fab repair manual that you can download in PDF format, or they will send it to you free of charge on a CD along with other info. If you're looking for a simple, self contained plating system, try Hunter Products at (908) 526-8440. They sell a self contained pen system (Micro Metallizer) that eliminates the mess of chemical bottles, have also had good luck with it. Mike McMonagle PCA Process Engineering Supervisor K*Tec Electronics 1111 Gillingham Lane Sugar Land, TX 77478 (281) 243-5639 Phone (281) 243-5539 Fax [log in to unmask] > -----Original Message----- > From: Stephen R. Gregory [SMTP:[log in to unmask]] > Sent: Tuesday, January 19, 1999 12:57 PM > To: [log in to unmask] > Subject: [TN] Assy: Source for Gold Plating Solution > > Hello out there! > > Remember my post last week about solder preforms for PC104 > connectors? > Remember what I was whining about? 'Bout the difficulty in hand > soldering > those things without getting solder on the gold plating? > > Well, you can guess what this email is about...I need some gold > plating > solution now. (BIG surprise there huh?) > > The source I used to get it from here in "Silicon Valley" has > disappeared...does anybody know of another source I can buy it from? > It would > be kinda' nice if it was here in the valley, but not nessesary. > > I'd sure appreciate it! > > -Steve Gregory- > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################