Rod, I can't answer your first question. For the second question, please contact Sherman Sum of Richey Electronics in Burnaby (420-0313). I currently use Chemtronics Twillwipes, p/n: C900. It does wonderful job of cleaning stencils and leave no wiper shreds, but I don't know if roller wiper version for automatic cleaning is availabe from Chemtronics. Give my regard to Sum. Matthew Park NII-Norsat International Inc. Surrey, BC. >>> Rod Lafond <[log in to unmask]> January 11, 1999 10:58 am >>> Actually I have two questions. 1) Does anyone have data showing the effect on solder joint reliability of a twice re-flowed BGA? A client is considering a board design with BGAs on both sides and is concerned about the reliability of the solder joints on a BGA placed on the first side because it would be exposed to two reflow cycles. Has anyone done this and followed up with any long term studies? Would a second application of flux be useful ? 2) This one is more straight-forward. Where can I buy a 'tack-roller' for cleaning solder paste from the bottom side of stencils? Even the best 'lint free' wipers tend to shear and leave tiny shreds on the stencil. Thanks in advance, Rod Lafond Manufacturing Engineering Aimtronics, Delta B.C. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################