I am need of any data supporting the use of URALANE 7760 jointly with a paste reflow process. Will the URALANE hold up in a reflow environment and is the green strength capable of holding high pin count devices in place prior to reflow. What is the method of application dispense or screen? Candace Garcia Group Technologies (813)972-6786 [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################