Brian ; if you really have a year old boards to store : get them interleaved (with raw brown desicating paper) and sealed . Boris may give you the source & how he does it . Beats sicabags and scraping boards against each other (with 3u" Au it helps) . See you paul klasek http://www.resmed.com > ---------- > From: Vascukynas, Brian[SMTP:[log in to unmask]] > Sent: Saturday, 9 January 1999 2:05 > To: [log in to unmask] > Subject: [TN] Bare PWB Packaging > > Hello, > > I am in the process of changing our Bare PWB Specs and would > like to change our Packaging requirements from suppliers. > > Unfortunately some of the PWB's we purchase end up sitting > on our stockroom shelves for over 6 months (In some cases more than > that) > > Currently are spec is weak at best and was wondering if anybody could > give me some good ideas. > > I would like to reference an IPC spec but am having a difficult time > finding > one. > > Thanks in advance > > Brian Vascukynas > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################