You might contact Harry Wachob at Exponent Failure Analysis... tel# (650) 688-7080 > Bill Davis, Ph.D. > Diamond Multimedia Systems > Senior Scientist > Tel. 408.325.7868 > Cell. 408.888.5650 > e-mail: [log in to unmask] > > -----Original Message----- From: Maguire, James F [mailto:[log in to unmask]] Sent: Wednesday, January 13, 1999 4:22 PM To: [log in to unmask] Subject: [TN] Dye Penetration Testing of BGA solder joints As part of our BGA reliability testing we would like to perform dye penetration testing of some of our BGA solder joints (typically after they've seen vibration and/or thermal stress tests.) I've seen references to dye penetration tests being done (and even photo's of joints); what I am looking for is a reference to a person that actually has done this. We've tried and frankly are having difficulties (with plastic BGAs) "popping off" the BGA to look at the solder joint. Typically, we tend to fail at the interface between the substrate (sometimes the PWB, sometimes the interposer) and the pad rather than in the solder joint. Now this happens EVEN on parts that have gone through extensive life testing (thermal cycle/shock) and gone "open". We've cross sectioned some parts and the solder joints (many of them) are in fact cracked. I have a feeling there is a "technique" to this and I want to talk first hand with a person that's "got the touch". Thanks for your assistance. -------------------------------------------------------- Jim Maguire Boeing Phantom Works E/E M&P Phone (253)657-9063 Fax (253)657-8903 email: [log in to unmask] --------------------------------------------------------- --------------------------------------------------------- Jim Maguire Boeing Phantom Works E/E M&P (253)657-9063 email: [log in to unmask] --------------------------------------------------------- ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################