Address, I have a 12 layer, 9 x 9, .062 PCA with 4 50mil pitch BGAs. Two (2) of the BGAs are normal 300+ IO perimeter and full array OMPACs. The other two are 500+ IO Perimeter BGAs with aluminum bodies. We suspected shorts on both packages and on several PCAs. An outside lab provided us some excellent and I mean excellent Radio Graph photos @ 80KV. We found the suspected shorts as well as solder ball voids, everywhere. The BGA pads are .025", again on .050" centers. I estimate some solder voids (air pockets) to be as great as .054" As a note, our design does have vias in the BGA pads, however, we have soldermasked the solder side for obvious reasons. Worst case voids do have vias in them. Voids are apparent all over. The same condition was not witnessed on the OMPACs. This condition is only witnessed on the Aluminum Package BGAs. I'm going to run some more thermal profiling on these BGAs only, but request the following from the group. 1. What advice can anyone provide on this problem. Any other angles are appreciated. 2. Are there any thermal profile considerations on these BGAs and what changes can be made without influencing changes to the OMPACs. 3. I'm using Convection Reflow. 4. Could the solder balls on the package be defective? I don't see this as being a problem. 5. I know the solder balls are not hygroscopic, so can moisture be creating these ball voids? Again, any input is appreciated. Thanks, John Gulley ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################