Hi Michael, You have received pretty good advice from Dave, Bill, Paul, and Andy, but the answer bill got from the 'head of all soldering operations at Siemens' is essentially non-information, if not dis-information. The properties change with composition, of course, but not wildly, and as far as fatigue reliability is concerned by about a factor of 2 to 3, which is small potatoes compared to the impact of other parameters determining the lives of solder joints. From your original question as well as your 2nd message, it is not clear why you want or need a high-temp solder. From your description of the clip-leads with solder preforms I am guessing that we are talking about NAS clip-leads and that you are using some ceramic components on FR-4 or polyimide. Depending on component size and severity of use conditions (as well as the compliancy of the lead geometry), your primary concern should most likely be the reliability of the solder joints. I have extensive experience with clip-leads and published the results of an exhaustive reliability study (Engelmaier, W., and A. I. Attarwala, "Surface- Mount Attachment Reliability of Clip-Leaded Ceramic Chip Carriers on FR-4 Circuit Boards," IEEE Trans. Components, Hybrids, and Manufacturing Technology, Vol. CHMT-12, No. 2, June 1989, p. 284), and there certainly is no problem with near eutectic Sn-Pb solder. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 904-437-8747, Fax: 904-437-8737 E-mail: [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################