Hi Tom - I don't have a total set of answers for you, but a few pointers which may fit with the inputs of others. 1] There are so many different urethane formulations that you need to query the specific material manufacturer regarding strippers. Urethanes tend to be rather tough materials and may be very difficult to strip without harm to other parts on the board, particularly if you have trimpots, switches, etc. I have good success desoldering individual components without removing coating, cleaning up the discolored coating and soldering in the replacement parts, followed by spot cleaning and patch coating. In general, the less you can do, the better. 2] Depends on the temperature and the material involved. At a minimum, I would be leery of reflow temperatures setting up some extreme stresses with the encapsulant. 3] Most clear urethane coatings turn a distinct amber, commencing at about 130deg.C. The manufacturer can best advise you on any loss of properties. Reflow temperatures may be close to the carbonization point for some of these materials. 4] Your cleaning method needs to be governed by the contaminant (what type of flux residues, etc.) and the geometry of the assembly. Dependent on the assembly and extent of work performed, simple spot cleaning may be adequate. Passing a fully assembled, partially conformal coated CCA thru an in line or diswasher cleaner does pose some risks. 5] At best, a conformal coating is a vapor permeable barrier. I would recommend that any form of overall fluid cleaning performed on a coated board be followed by a dehumidification cycle in an air circulating oven at whatever temperature the components will stand. If you happen to apply conformal coating over moisture or contaminants, it will become apparent by the formation of tiny bubble clusters following a bit of environmental testing. Good luck - Kelly ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################