Lik-Jen Wu, In one of my former lives working as a Senior Manufacturing Engineer for a Fortune 100 Company, I ran into the same problem... lots of shorts on PGA packages. We solved this problem by "rotating" the PCB 45 Degrees to the wave, thereby increasing the effective distance pin to pin by 41%. This can be accomplished by either: 1: Rotate the solder pot in your machine (very difficult) 2: Buy a machine that has the pot at 45 deg (very expensive) 3: Design and build pallets to hold the board at 45 deg. (very time consuming) 4: Buy pallets that can do this (we make them here, but I do not want to advertise). One caveat with using pallets is the width of your soldering machine... these guys get pretty large. Contact me "off-net" if you'd like to discuss this further. Regards, Ed Popielarski QTA Machine 10 Mc Laren, Suite D Irvine, Ca. USA 92618 Ph: (949)581-6601 Fx: (949)581-2448 E-Mail: [log in to unmask] http://www.qta.net ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################