If you mean dielectric thickness - TDR, in conjunction with destructive testing (x-section), is the only test method providing objective evidence. All required factors are then capable of being corelated (thickness confirmed, trace width, Dk, etc.) and confirmed. Earl Moon ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################