Phil, I forgot to mention that these are PTH boards. Thanks, KennyB At 09:54 AM 12/15/98 -0800, Crepeau, Phil wrote: >hi, > >try paragraph 6.5.3. > >phil crepeau > >-----Original Message----- >From: Kenny Bloomquist [mailto:[log in to unmask]] >Sent: Tuesday, December 15, 1998 7:53 AM >To: [log in to unmask] >Subject: [TN] Lead Protrusion > > >I am trying to find the lead protrusion requirements in J-STD-001. Either >I'm missing it or it "ain't" there. IPC-A-610 says visible to 1.5mm but >can't find it in 001. > >Thanks, > >Ken Bloomquist >Sr. Principal Process Engineer >PRIMEX Aerospace Company >P.O. Box 97009 >Redmond, WA 98073-9709 >www.primextech.com > >Ph: 425-885-5000 >FAX: 425-882-5786 >[log in to unmask] > >Northcon/98, Show Director ><www.northcon.org> > >Electronics Manufacturers Association (EMA), Secretary ><www.ema-wa.org> > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section >for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or >847-509-9700 ext.312 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################