Dear Mr. Doty:
We have employed two methods to measure the gold, gravimetric and AA.
The gravimetric method is consistantly superior (at least within our
lab) in accuracy when RSD and % recovery of a known data were
evaluated.
I understand your concern, as acidification of the gold sample results
in the evolution of hydrogen cyanide gas. Typlically, the sample size
is small though (< 10 ml) with either the gravimetric or AA method.
Wish I could be of more help.
Regards,
Ted Stern
Michael D. Doty wrote:
>
> Hello Techies,
>
> I have a couple of questions on gold bath analysis. We
> currently use the gold prospector from Dynatronix. Since they are no
> longer making these nor supplying test solutions I was wondering what
> the alternatives might be. I know of the gravimetric method utilizung
> Nitric and Sulfuric acids but my Lab operators have some major
> heartburn with this.
> Thanks in advance for the help.
>
> Mike Doty
> Process Eng.
> Hadco TCE
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################