Try the laboratory supply houses like VWR Scientific Products (1-800-932-5000), or JT Baker(1-800-JTBAKER) for "Baker Test Strips" They have a lot of different specific ion test strips. > -----Original Message----- > From: Teo Tijerina [SMTP:[log in to unmask]] > Sent: Thursday, December 17, 1998 3:59 PM > To: [log in to unmask] > Subject: [TN] Looking for Silver Chromate Paper to use for IPC-TM-650 > > Ladies & Gentlemen: > I am trying to initiate test IPC-TM-650 in my wave solder machine to > test for the presence of halides in a "halide-free" no clean flux. I have > had issues with cross contamination of water soluble and no clean flux due > to operator error (ie. the operator accidentally dumps water soluble flux > into a no clean flux bath). IPC-TM-650 calls for the use of silver > chromate test paper. Does anybody know where I can get some of this > paper? > Anybody have any ideas on how to prevent cross contamination of fluxes > > -Thanks, > > Teo Tijerina > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################