Dynachem makes a good film for gold plating. Of course the better films for adhesion are also harder to develop completely & to strip off later. Their 500 series film is good for gold. ______________________________ Reply Separator _________________________________ Subject: [TN] Problem in Gold Plating Author: <[log in to unmask] > at INTERNET-OWEGO Date: 11/6/98 5:22 PM I work in gold plating. We are using electrolytic gold plating. It is pattern plating. However the gold leaks underneath the dry film. As a result the pattern is fatter after the dry film is removed. We develop the pattern dry film and thenn hardenn the dry film by exposing under UV light again. But still it leaks underneath the dry film. Could any one help ? WE also want to set up a pulse plating bath ourselves. Could any one give us some information onn how to start ? Thanks in advance!!!!!!!! my e-mail : [log in to unmask] ( Please do not send graphics, this is text base) Thanks again Francis ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text n the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for ditional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 t.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################