In a message dated 98-11-25 18:53:46 EST, you write: << We beleive this tin oxide is not soluble True, in water... and can not be cleaned with any thing, Not true, but what it may need to be cleaned in may be unacceptable... and in order to eliminate this tin oxide residue we must eliminate oxygen in the assembly process and use Nitrogen (N2). Eliminating Oxygen should eliminate the problem... The residue you are seeing is either an insoluble Stannous Tin compound, likely an organic Stannous compound, or it is (more likely) Stannic Tin oxide. Either compound requires an alkaline cleaner to COMPLETELY remove it. (Some organic solvents may partially, or largely remove it) The Stannic Tin oxide can be removed by either a STRONGLY alkaline cleaner, basically dilute Caustic, or dilute Hydrofluoric Acid, or Ammonium Bifluoride (which really is half neutralized Hydrofluoric Acid). If removal is the path you want to take, rather than prevention, get back to me directly, and we can discuss specific options. Rudy Sedlak RD Chemical Company ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################