Kinnarney Rubber Company (609-468-1320) makes masking boots for conformal coat and probably has something for hole plugs too.... Mike McMonagle PCA Process Engineering Supervisor K*Tec Electronics 1111 Gillingham Lane Sugar Land, TX 77478 (281) 243-5639 Phone (281) 243-5539 Fax [log in to unmask] > -----Original Message----- > From: <Jason M. Smith> [SMTP:[log in to unmask]] > Sent: Tuesday, November 03, 1998 10:50 AM > To: [log in to unmask] > Subject: Re: [TN] hole plug source > > Does anyone have a source for wave soldering tooling hole plugs? The > company we > were sourcing from went out of business and we've been reluctant to > find another > supplier. The plugs are a soft rubbery grommet like materials easily > applied > and removed to protect solder from going up through the holes and the > air knife > to blow unnecessarily through holes that are approx. 1/4" in diameter, > but the > material is to flexible enough to accomodate sizes in the same > neighborhood. I > would appreciate your assistance. > > Jason Smith > process materials engineer > Lexmark Electronics > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################