Rudolph, Please check old responses to this question in the Technet archives. Short answer; there are no pass/fail criteria for this test for no clean fluxes as many of the ions detected by this methods are from the dissociation of carboxylic acids, rather than (I guess this answer isn't so short after all) the nastier halides or sulphate. What you can do with this test for no-cleans is find out whether you are giving your boards a flux bath - use it as a green/yellow light, rather than a green/red light. regards, Bev Christian Nortel > ---------- > From: Rudolph Yu[SMTP:[log in to unmask]] > Sent: Wednesday, November 11, 1998 12:19 PM > To: [log in to unmask] > Subject: [TN] need test lab for no clean process > > Does anyone know if there is a test lab in San Jose,CA which can test > for the ionic contamination level on assembly? > Also do you think I should use the 10.06 mg NaCl/ in^ as the limit for > a no clean process? > > Thank you for reading this mail > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################