send me your fax number, I'll send a chart Alex fax (612) 721-5311 -----Original Message----- From: Scott Holthausen <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: Tuesday, October 13, 1998 4:47 PM Subject: [TN] Copper Question >Hello Technetter's > >Roughly, how thick is 1oz. copper? How about .5oz. copper? I can't seem to >remember how the equation goes. > >Thanks, >Scott Holthausen > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################