Hi Dr.Smith! Blakening process means black oxide prcocess. Braun process means brown oxide process. Electrolytic plating process I think Electroless plating process is correct. This process is also one of the adhesion promoting copper surface treatment for multilayer bonding. Electroless copper plating or electroless Ni plating are used instead of black or brown copper oxide. Copper oxide reduction process has developed to prevent "Pink Ring". CuO is reducing to Cu or Cu2O by reducing agent "DMAB". DMAB:Dimethyl Amine Borane Electroless copper platig process is also "Non Pink Ring" process. Regards, Motoyo Wajima General Purpose Computer Division,Hitachi Ltd.(Japan) Dr. Warren Smith $B$5$s$O=q$-$^$7$? (B: >Yet another question from your friendly neighborhood Japanese translator... > >In this test I am translating, there is a question I have translated as >follows: > >7. Which of the following is not appropriate as an inner-layer pattern >surface treatment method? > i. Blackening process > ii. Braun process > iii Electrolytic plating process > iv. Copper oxide reduction process > > >My questions are as follows: 1) Is it "Braun" or "Brown" for ii. 2) What is >the blackening (or darkening) process? > >Thanks! > >Warren > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > *********************************************** Motoyo Wajima General Purpose Computer Division,Hitachi,Ltd. 1 Horiyamashita Hadano-shi,Kanagawa-ken,259-13 Japan E-mail:[log in to unmask] Fax:+81-463-88-2935 *********************************************** ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################