Hi everyone, I just thought of something else that might work. Since the pads are thru-hole, can I just place the component on top and run it through wave? Since the pads are plated thru-hole, solder will come up and create a joint with BGA balls. Any input would be greatly appreciated. Tom Han Ardent Systems ___________________________________________________________________ You don't need to buy Internet access to use free Internet e-mail. Get completely free e-mail from Juno at http://www.juno.com or call Juno at (800) 654-JUNO [654-5866] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################