Technetters, This is the second time I have asked this question but so far I haven't had a reply. Maybe I'll ask in a different way this time! We are trying to solder a microswitch to a PCB and are having serious problems with dry joints (i..e de-wetting of the legs). Having spoken with the supplier of the switch he has informed me that the switch legs(there are two of them) have different platings these are: Material: CuZn37-F37 Finish: 2 microns Silver Plated. Nominal 0.2 microns gold. and Material: CuZn37-F37 Finish : Nominal 0.2 microns gold My questions are: What does the silver do to solderability? Why would a switch manufacturer use these finishes? Should the second leg have a barrier layer (Nickel?) between the brass and the gold? My swich supplier is willing to listen but what would be the best finish for us to solder whilst meeting the switch manufacturers requirements? HELP!!!! Neil Atkinson ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################