Kelly and Technetters, I discovered and error in my earlier post. The corrected post is below. Correction is in caps. Try this method which is recommended by a large pcb fabricator. We are about to give it a try on one of our designs. Create 2 sets of masking artwork; the LPI artwork, and the plug artwork. For the LPI artwork make the via aperture the same size as the drilled hole (.005 larger then nom. FHS) on the solder side, and .006 larger than drilled hole on the component side. For the plug artwork, use a .012 aperture LARGER THAN THE DRILLED HOLE. Specify "plugging" to be done from the solder side with a wet solder mask, and after solder leveling. Via reliability is enhanced because the solder in the barrel acts as an oxide inhibitor. By creating "via plug" artwork, you can define test and non-test vias which are left open for probing. Tom Hybiske General Atronics Corp. 1200 E. Mermaid Lane Wyndmoor, PA 19038 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################