Paul; The answer to your question is both can be the problem. Cleanliness is a real issue and the plastic has low surface energy in relation to the conformal coating. Manufacturers of these coating are working all the time to improve overall adhesion. This is not as simple a problem as it might seem. There are many issues to deal with and not all are apparent to the end user. -----Original Message----- From: Paul Stolar <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: Monday, October 12, 1998 9:19 AM Subject: [TN] Confomal coating adhesion > Does anyone have any good experience at improving conformal coating > adhesion to plastic packaging? > > Is it a cleanliness issue, or is it inherent in materials? > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################