Hi Tim, Yes, we have tried that approach ....we even have made some of our designs like that at your facility.... the olnly issue there is the additional standoff, especially that close to the BGA pads and less than 0.025" SMT ...that definitely affects the solder print resolution/process....let me know if you can think of any other 'relatively inexpensive' way of doing this.... Marcelo -----Original Message----- From: Tim Snodgrass [SMTP:[log in to unmask]] Sent: Thursday, October 22, 1998 6:12 PM To: TechNet E-Mail Forum.; Chan, Marcelo Subject: Re: [TN] Plugged/tented vias Marcelo We have used a two step soldermask process to tent vias. First we put a layer of dryfilm down and print it with via image. Then coat the board with liquid soldermask. Then print that image. This produces a part with tinted via's and liquid photoimageable to ensure that there is no entrapment in the via holes. If you have any questions contact me off line. Regards, Tim Snodgrass Young Electronics 818 407-4024 Chan, Marcelo wrote: > We have tried different approaches to tenting/plugging vias for BGA and some > backplane applications using LPI and screened SM with limited success...PWB > vendors claim they could do it, but we are still looking for some one who could > do this on 100% of the vias with no pin holes and it has to be done on both > sides to prevent entrapment of cleaning solutions...the via sizes that we have > in mind can have a finished hole diameter as large as 22 and as small as 13 > mils...Can someone share their 'hands-on' experiences on this issue with me > through Technet or even off-line? > Thanks > > Marcelo Chan > Lead Engineer - Advanced Manufacturing Technology > Electronics Systems Sector, Harris Corp., FL > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################